Sem/edx services in Chelmsford, MA

Sem/edx services in Chelmsford, MA

Microhardness testing company in Chelmsford? Energy Dispersive Spectroscopy (EDS) identifies the elements present in a sample by analyzing the X-rays generated by the electron beam of the Scanning Electron Microscope (SEM), making it an indispensable tool. Since X-rays are only generated from the area of the surface excited by the small electron beam, spectra of individual areas or particles can be obtained. Spectral information can therefore be generated for an entire field of view by scanning the beam, providing an elemental map. With the high count rate and excellent signal to noise ratio of our advanced QDD EDS detectors, high resolution data sets are collected and analyzed in minutes, rather than days. This elemental mapping technique allows our clients to immediately visualize the chemical landscape in their samples. Additionally, since the entire spectra is stored for each pixel, areas of interest that are identified later can be examined in detail, without ever having to re-image the sample. Other labs can’t touch the quality and visual impact of the elemental maps we produce here at MicroVision Labs. See additional info on ftir laboratory.

Problem: A client was a manufacturer of beverages, bottled water, and other drinks. They received a customer complaint through one of their distributors, which indicated that a customer had been drinking a bottle of water, and as they neared the bottom of the bottle, found a mysterious white powder floating in the bottom. The customer returned the bottle and complained. The client hoped to identify the powder so they could both satisfy their end customer, as well as identify any potential problems in their manufacturing or bottling process.

MicroVision Laboratories’ analytical experts were able to meet with the QC Engineers and develop an analytical plan as to which solder joints to cross section and inspect. The client not only wanted to determine if there were any significant issues with the solder joint but also determine that there was a good intermetallic bond between the tin/lead solder and the copper wires of the chip packages.

What is your standard turnaround time (TAT) and can it be expedited? Our standard TAT is 5 to 10 business days. We can provide faster TATs on request with the following surcharges: – Same day to 24 hour rush is 100% surcharge – 2 day rush is 75% surcharge – 3 day rush is 50% surcharge – 4 day rush is 25% surcharge Rush requests must have prior approval otherwise we cannot guarantee turnaround times.

The client was able to determine the source of the black dust was due to the mechanical breakdown of the foam cushions in the impacted room, and not from mold or mildew growth. The experienced analysts at MicroVision Labs were able to differentiate the foam materials from either blown cellulose or urethane foam insulation or air filters, allowing for the client to easily remove the problem cushions.

?We partner with companies in all phases of product development and sales, including R&D, manufacturing, QC, advertising and failure analysis. Our laboratory offers a highly-trained and experienced staff utilizing a powerful set of analytical tools (SEM with EDS and backscatter detectors, Bruker X-Flash elemental mapping, X-Ray imaging, Micro-FTIR spectroscopy, Micro-XRF, light microscopy, cross sectioning/precision polishing and microhardness testing). See extra info on https://microvisionlabs.com/.